Polymer Property : Vicat Softening Point = 44.4 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 44.4 °C
112 °F
ASTM D1525
ExxonMobil OPTEMA™ TC 130 Molding, extrusion and compounding resin  (discontinued **)
OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and..
Vicat Softening Point 44.4 °C
112 °F
ASTM D1525
ExxonMobil Escorene™ UL 00328 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00328 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applications: Compoun..
Vicat Softening Point 44.4 °C
112 °F
ASTM D1525
ExxonMobil Escorene™ FL 00328 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00328 is a copolymer of ethylene and vinyl acetate offering low gel. Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation. Machine..