ExxonMobil Escorene™ FL 00328 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ FL 00328 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: FL 00328 is a copolymer of ethylene and vinyl acetate offering low gel. Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation. Machines should always be completely purged with LDPE or suitable cleaning compound before shutdown. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No Applications:Co-Extrusion FilmsCompoundingFabric CoatingSheet ExtrusionInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ExxonMobil method
Vinyl Acetate Content 27 %
27 %
ExxonMobil method
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 81

@Time 15.0 sec
81

@Time 0.00417 hour
Molded Properties; ISO 868
Tensile Strength at Break >= 0.689 MPa
>= 100 psi
Molded Properties; ISO 527-2/1A/100
Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2/1
Thermal Properties Metric English Comments
Melting Point <= 160 °C
<= 320 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 44.4 °C
112 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 220