Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 168.7 °C | 335.7 °F | 10 N; ASTM D1252 |
CRP Technology Windform® GF 2.0 Polyamide-Aluminum-Glass Composite Processed by selective laser sintering (SLS). Windform® GF 2.0 is the evolutionary substitute for Windform GF, our first generation material. Windform® GF 2.0 is a composite material made of poly.. |