Thermal Properties Metric English Comments
Vicat Softening Point 168.7 °C
335.7 °F
10 N; ASTM D1252
CRP Technology Windform® GF 2.0 Polyamide-Aluminum-Glass Composite
Processed by selective laser sintering (SLS). Windform® GF 2.0 is the evolutionary substitute for Windform GF, our first generation material. Windform® GF 2.0 is a composite material made of poly..