Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 98.9 - 166 °C | 210 - 331 °F | Average value: 150 °C Grade Count:29 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Vicat Softening Point | 98.9 - 166 °C | 210 - 331 °F | Average value: 154 °C Grade Count:8 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |