Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 60.0 - 143 °C | 140 - 289 °F | Average value: 122 °C Grade Count:22 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |