Polymer Property : Vicat Softening Point = 262 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 84.0 - 128 °C
183 - 262 °F
Average value: 91.9 °C Grade Count:44
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..