Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite Optix® CA - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite Optix® CA - 1000 E-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite Optix® CA - 1000 I High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite Optix® CP - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite Optix® CP - 1000 I High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 1000 I High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite West Optix® CP - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 1000 E-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 108 °C | 227 °F | Rate A (50°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hyrene® PSCRY 1.5 General Purpose Polystyrene Available in North America Features: Crystal, High Heat Resistance, General Purpose, High Molecular WeightRoHS Compliant Form: Pellets Information provided by Entec |
|||
Vicat Softening Point | 108 °C | 227 °F | Rate B (120°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |
|||
Vicat Softening Point | 108 °C | 227 °F | Rate B (120°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hyril® SAN500 Styrene Acrylonitrile Available in North America Features: Copolymer Form: PelletsInformation provided by Entec |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D1525 |
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsFoamOPSMedicalInformation provided by AmericasSty.. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D1525 |
Americas Styrenics STYRON® 685DL High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantTypical ApplicationsFoamOPSMedicalInformation provided by AmericasStyrenics LLC. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D1525 |
Americas Styrenics STYRON® 665 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeFood Contact CompliantTypical ApplicationsFilmInformation provided by AmericasStyrenics LLC. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D1525 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite West Optix® CP - 1000 I High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |