Polymer Property : Vicat Softening Point = 218.5 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 103.6 °C
218.5 °F
ISO 306
Tisan TISSAN® UNR Styrene Acrylonitrile
Properties:Natural or ColoredGlass fiber and glass beadMineral filledFlame retardantGood thermal and chemical resistanceExcellent transparencyExcellent mechanical propertiesDimensional stabilityEasy..