Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 87.2 - 91.1 °C | 189 - 196 °F | ASTM D1525 |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 88.0 - 91.0 °C @Temperature 120 - 120 °C |
190 - 196 °F @Temperature 248 - 248 °F |
Average value: 89.7 °C Grade Count:3 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Vicat Softening Point | 63.0 - 91.0 °C | 145 - 196 °F | Average value: 76.4 °C Grade Count:30 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |