Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 168 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific)
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East)
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer
EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 168 °C
334 °F
50°C/h 50N
Covestro Apec® 1705 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr..
Vicat Softening Point 168 °C
334 °F
50°C/h 50N
Covestro Apec® DP 1-9349/5 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
Vicat Softening Point 168 °C

@Load 1.00 kg,
Thickness 4.00 mm
334 °F

@Load 2.20 lb,
Thickness 0.157 in
ISO 306
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound  (discontinued **)
Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall..
Vicat Softening Point 168 °C

@Load 1.00 kg,
Thickness 4.00 mm
334 °F

@Load 2.20 lb,
Thickness 0.157 in
ISO 306
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound  (discontinued **)
Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
Vicat Softening Point 168 °C
334 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 168 °C
334 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Vicat Softening Point 168 °C
334 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Vicat Softening Point 168 °C
334 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Vicat Softening Point 168 °C
334 °F
Covestro Apec® HT KU 1-9340/5 High-Heat Polycarbonate
Transparent and opaque shades possible, easy-to-demold.Applications: Medical sector: superheated steam sterilization.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was s..
Vicat Softening Point 168 °C

@Load 1.02 kg
334 °F

@Load 2.25 lb
ISO 306
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Vicat Softening Point 168 °C
334 °F
50°C/h 50N
Covestro Texin® 255 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop..
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL FE8000S PPE+PS
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
Vicat Softening Point 168 °C
334 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
Copyright © lookpolymers.com All Rights Reserved