Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 78.0 - 155 °C | 172 - 311 °F | Average value: 147 °C Grade Count:35 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Vicat Softening Point | 150 - 155 °C | 302 - 311 °F | Softening point range is 150-155°C. Method not specified. |
Total PPH 3762 Polypropylene, Extrusion Grade Homopolymer fiber grade for staple fiber and multifilament yarnsFading Resistance - FINA 3762 is formulated to resist gas fading while maintaining excellent processing stability up to 250oC.Process .. |
|||
Vicat Softening Point | 50.0 - 155 °C | 122 - 311 °F | Average value: 112 °C Grade Count:25 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |