Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 51.7 °C
125 °F
ASTM D1525
ExxonMobil Escorene™ FL 00623 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00623 is a good coextrusion partner in extrusion coating, blown and cast film. Excellent sealing material with a very low seal initiation temperature. Availability: Africa & ..