Polymer Property : Vicat Softening Point = 118 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 48.0 °C
118 °F
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica..
Vicat Softening Point 48.0 °C
118 °F
Rate B; ASTM D1525
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Vicat Softening Point 48.0 °C
118 °F
Rate B; ASTM D1525
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Vicat Softening Point 48.0 °C
118 °F
1000g; ASTM D-1525
ExxonMobil Escorene® LD-761 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer designed for high filler acceptance. Compounds produced from this resin have excellent flexibility and toughness.Appl..
Vicat Softening Point 48.0 °C
118 °F
1000g; ASTM D-1525
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile..
Vicat Softening Point 48.0 °C
118 °F
Rate B, ASTM D1525-70
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc  (discontinued **)
Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc..
Vicat Softening Point 48.0 °C
118 °F
ISO 306
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer
Type: Pearlthane® D91F88 is an aliphatic-based thermoplastic polyurethane.Main Application : ExtrusionSpecial features : Outstanding abrasion loss, excellent color stability upon weather exposure..
Vicat Softening Point 48.0 °C
118 °F
VST/B/50; ISO 306
Styrolution Styrolux® 693 D SBC
Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e..
Vicat Softening Point 48.0 °C
118 °F
ASTM D1525
DuPont Bynel® 3860 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Vicat Softening Point 48.0 °C
118 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill..
Vicat Softening Point 48.0 °C
118 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent ..
Vicat Softening Point 48.0 °C
118 °F
B (50N); ISO 306
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed..
Vicat Softening Point 48.0 °C
118 °F
ASTM D1525, ISO 306
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Vicat Softening Point 48.0 °C
118 °F
ASTM D1525, ISO 306
DuPont™ Surlyn® 9320 Zinc Ionomer
Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin ..
Vicat Softening Point 47.8 °C
118 °F
ASTM D1525
ExxonMobil OPTEMA™ TC 120 Molding Ethylene Methyl Acrylate
Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE..
Vicat Softening Point 47.8 °C
118 °F
ASTM D1525
ExxonMobil Polybilt™ Bitumen Modifier 101 Low Density Polyethylene Resin
Product Description: Polybilt 101 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 10..
Vicat Softening Point 47.8 °C
118 °F
ASTM D1525
ExxonMobil Escorene™ 768.MJ Blown Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 768.MJ is a low gel 26.2% vinyl acetate copolymer designed for film and compounding applications. This resin provides very low modulus films with high tensile ..
Vicat Softening Point 48.0 °C

@Load 1.02 kg
118 °F

@Load 2.25 lb
ASTM D1525
Arkema Group LOTRYL® 20 MBG 08 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 20MBG08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MBG 08 is a polyme..
Vicat Softening Point 48.0 - 90.0 °C
118 - 194 °F
Average value: 74.4 °C Grade Count:12
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an..