Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 88.0 - 104 °C | 190 - 219 °F | Average value: 93.5 °C Grade Count:5 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Vicat Softening Point | 88.0 - 104 °C | 190 - 219 °F | Average value: 95.9 °C Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |
|||
Vicat Softening Point | 80.0 - 104 °C | 176 - 219 °F | Average value: 92.4 °C Grade Count:73 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |