Mechanical Properties Metric English Comments
Shear Modulus 0.593 GPa

@Temperature 100 °C
86.0 ksi

@Temperature 212 °F
DAM; ISO 6721
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Shear Modulus 0.593 GPa

@Temperature 160 °C
86.0 ksi

@Temperature 320 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and..