Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.4857 GPa @Temperature 70.0 °C |
70.45 ksi @Temperature 158 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |