Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 31.0 GPa @Temperature 300 °C |
4500 ksi @Temperature 572 °F |
Condition T6x (Quench in water at RT) |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Shear Modulus | 31.0 GPa @Temperature 250 °C |
4500 ksi @Temperature 482 °F |
Condition T6x (Quench in water at RT) |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Shear Modulus | 31.0 GPa @Temperature 250 °C |
4500 ksi @Temperature 482 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Shear Modulus | 31.0 GPa @Temperature 300 °C |
4500 ksi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Shear Modulus | 31.0 GPa @Temperature 300 °C |
4500 ksi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Shear Modulus | 31.0 GPa @Temperature 20.0 °C |
4500 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Shear Modulus | 31.0 GPa @Temperature 20.0 °C |
4500 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |