Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Modulus = 437.6 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 3.017 GPa

@Temperature -50.0 °C
437.6 ksi

@Temperature -58.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and..
Copyright © lookpolymers.com All Rights Reserved