Mechanical Properties Metric English Comments
Shear Modulus 28.0 GPa

@Temperature 150 °C
4060 ksi

@Temperature 302 °F
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F
Information provided by PEAK Werkstoff GmbH
Shear Modulus 28.0 GPa

@Temperature 20.0 °C
4060 ksi

@Temperature 68.0 °F
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Shear Modulus 28.0 GPa

@Temperature 150 °C
4060 ksi

@Temperature 302 °F
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F
Information provided by PEAK Werkstoff GmbH
Shear Modulus 28.0 GPa

@Temperature 20.0 °C
4060 ksi

@Temperature 68.0 °F
Condition T6
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4
High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH