Polymer Property : Shear Modulus = 3920 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 27.0 GPa

@Temperature 200 °C
3920 ksi

@Temperature 392 °F
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F
Information provided by PEAK Werkstoff GmbH
Shear Modulus 27.0 GPa

@Temperature 200 °C
3920 ksi

@Temperature 392 °F
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F
Information provided by PEAK Werkstoff GmbH