Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 27.0 GPa @Temperature 200 °C |
3920 ksi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Shear Modulus | 27.0 GPa @Temperature 200 °C |
3920 ksi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |