Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.275 GPa @Temperature 120 °C |
39.9 ksi @Temperature 248 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Shear Modulus | 0.275 GPa @Temperature 120 °C |
39.9 ksi @Temperature 248 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |