Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.220 GPa @Temperature 68.0 °C |
31.9 ksi @Temperature 154 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |