Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.66 GPa @Temperature -20.0 °C |
241 ksi @Temperature -4.00 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |