Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 24.0 GPa @Temperature 300 °C |
3480 ksi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Shear Modulus | 24.0 GPa @Temperature 200 °C |
3480 ksi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Shear Modulus | 24.0 GPa @Temperature 250 °C |
3480 ksi @Temperature 482 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Shear Modulus | 24.0 GPa @Temperature 300 °C |
3480 ksi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Shear Modulus | 24.0 GPa @Temperature 200 °C |
3480 ksi @Temperature 392 °F |
Condition T6 |
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Shear Modulus | 24.0 GPa @Temperature 250 °C |
3480 ksi @Temperature 482 °F |
Condition T6 |
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |