Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.49 GPa @Temperature -50.0 °C |
216 ksi @Temperature -58.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)