Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.1393 GPa @Temperature 150 °C |
20.20 ksi @Temperature 302 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |