Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.171 GPa @Temperature -20.0 °C |
169.8 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |