Mechanical Properties Metric English Comments
Shear Modulus 1.171 GPa

@Temperature -20.0 °C
169.8 ksi

@Temperature -4.00 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..