Mechanical Properties Metric English Comments
Shear Modulus 0.935 GPa

@Temperature -50.0 °C
136 ksi

@Temperature -58.0 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers