Mechanical Properties Metric English Comments
Shear Modulus 0.0781 GPa

@Temperature 160 °C
11.3 ksi

@Temperature 320 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers