Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.704 GPa @Temperature 70.0 °C |
102 ksi @Temperature 158 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Shear Modulus | 0.700 GPa @Temperature 250 °C |
102 ksi @Temperature 482 °F |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Shear Modulus | 0.700 GPa @Temperature 250 °C |
102 ksi @Temperature 482 °F |
|
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Shear Modulus | 0.700 GPa @Temperature 200 °C |
102 ksi @Temperature 392 °F |
ISO 6721 |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |