Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.56 GPa @Temperature -20.0 °C |
226 ksi @Temperature -4.00 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)