Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 92.0 MPa @Temperature 23.0 °C |
13300 psi @Temperature 73.4 °F |
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg IM2-C Fibre 1947 - 38% resin weight with IM2-C 53% fiber volumeInformation provided by HexCel |