Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg IM2-C Fibre

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg IM2-C Fibre.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1947 - 38% resin weight with IM2-C 53% fiber volumeInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2326 MPa

@Temperature 23.0 °C
337400 psi

@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D3039
Tensile Modulus 153 GPa

@Temperature 23.0 °C
22200 ksi

@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D3039
Shear Strength 44.0 MPa

@Temperature 60.0 °C
6380 psi

@Temperature 140 °F
0º Interlaminar Shear, Conditioning: 60°C-90%RH; ASTM D2344
63.0 MPa

@Temperature 90.0 °C
9140 psi

@Temperature 194 °F
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344
92.0 MPa

@Temperature 23.0 °C
13300 psi

@Temperature 73.4 °F
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F