Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 90.3 MPa @Temperature 104 °C |
13100 psi @Temperature 220 °F |
+/- 45° In-Plane, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |