Mechanical Properties Metric English Comments
Shear Strength 8.55 MPa

@Time 86400 sec
1240 psi

@Time 24.0 hour
Overlap, Maple
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Shear Strength 8.55 MPa

@Temperature -40.0 °C
1240 psi

@Temperature -40.0 °F
Overlap, Lexan, Substrate Failure
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 8.55 MPa

@Temperature -40.0 °C
1240 psi

@Temperature -40.0 °F
Overlap, Lexan, Substrate Failure
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 8.55 MPa

@Temperature -40.0 °C
1240 psi

@Temperature -40.0 °F
Overlap, Lexan, Substrate Failure
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..