Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.55 MPa @Time 86400 sec |
1240 psi @Time 24.0 hour |
Overlap, Maple |
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Shear Strength | 8.55 MPa @Temperature -40.0 °C |
1240 psi @Temperature -40.0 °F |
Overlap, Lexan, Substrate Failure |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 8.55 MPa @Temperature -40.0 °C |
1240 psi @Temperature -40.0 °F |
Overlap, Lexan, Substrate Failure |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 8.55 MPa @Temperature -40.0 °C |
1240 psi @Temperature -40.0 °F |
Overlap, Lexan, Substrate Failure |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |