Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.27 MPa @Temperature 177 °C |
1200 psi @Temperature 351 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp Formula is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids,.. |
|||
Shear Strength | 8.27 MPa @Temperature 24.0 °C |
1200 psi @Temperature 75.2 °F |
Overlap, Abraded and Solvent Wiped Steel |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 8.27 MPa @Temperature 24.0 °C |
1200 psi @Temperature 75.2 °F |
Overlap, Abraded and Solvent Wiped Steel |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 8.27 MPa @Temperature 24.0 °C |
1200 psi @Temperature 75.2 °F |
Overlap, Abraded and Solvent Wiped Steel |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 8.27 MPa @Temperature -55.0 °C |
1200 psi @Temperature -67.0 °F |
Overlap |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Shear Strength | 8.27 - 8.62 MPa @Temperature -55.0 °C |
1200 - 1250 psi @Temperature -67.0 °F |
Overlap Al/Al (etched); ASTM D1002-72 |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Shear Strength | 8.27 MPa @Temperature -55.0 °C |
1200 psi @Temperature -67.0 °F |
Overlap |
3M Scotch-Weld™ DP270 Clear Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Shear Strength | 8.27 - 8.62 MPa @Temperature -55.0 °C |
1200 - 1250 psi @Temperature -67.0 °F |
Overlap Al/Al (etched); ASTM D1002-72 |
3M Scotch-Weld™ DP270 Clear Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |