Polymer Property : Shear Strength = 1200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 8.27 MPa

@Temperature 177 °C
1200 psi

@Temperature 351 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp Formula is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids,..
Shear Strength 8.27 MPa

@Temperature 24.0 °C
1200 psi

@Temperature 75.2 °F
Overlap, Abraded and Solvent Wiped Steel
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 8.27 MPa

@Temperature 24.0 °C
1200 psi

@Temperature 75.2 °F
Overlap, Abraded and Solvent Wiped Steel
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 8.27 MPa

@Temperature 24.0 °C
1200 psi

@Temperature 75.2 °F
Overlap, Abraded and Solvent Wiped Steel
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 8.27 MPa

@Temperature -55.0 °C
1200 psi

@Temperature -67.0 °F
Overlap
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Shear Strength 8.27 - 8.62 MPa

@Temperature -55.0 °C
1200 - 1250 psi

@Temperature -67.0 °F
Overlap Al/Al (etched); ASTM D1002-72
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Shear Strength 8.27 MPa

@Temperature -55.0 °C
1200 psi

@Temperature -67.0 °F
Overlap
3M Scotch-Weld™ DP270 Clear Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Shear Strength 8.27 - 8.62 MPa

@Temperature -55.0 °C
1200 - 1250 psi

@Temperature -67.0 °F
Overlap Al/Al (etched); ASTM D1002-72
3M Scotch-Weld™ DP270 Clear Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M