Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 79.3 MPa @Temperature 121 °C |
11500 psi @Temperature 250 °F |
In-Plane, Wet; 270°F Oven Cure, 350°F Postcure; ASTM D3518 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Shear Strength | 79.3 MPa @Temperature -53.9 °C |
11500 psi @Temperature -65.0 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Shear Strength | 79.3 MPa @Temperature 82.0 °C |
11500 psi @Temperature 180 °F |
Short Beam, Dry |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |