Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 79.3 MPa

@Temperature 121 °C
11500 psi

@Temperature 250 °F
In-Plane, Wet; 270°F Oven Cure, 350°F Postcure; ASTM D3518
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Shear Strength 79.3 MPa

@Temperature -53.9 °C
11500 psi

@Temperature -65.0 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Shear Strength 79.3 MPa

@Temperature 82.0 °C
11500 psi

@Temperature 180 °F
Short Beam, Dry
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Information provided by HexCel
Shear Strength 79.0 MPa

@Temperature 177 °C
11500 psi

@Temperature 351 °F
T300; In Plane; Wet condition
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel