Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 52.4 MPa @Temperature 82.2 °C |
7600 psi @Temperature 180 °F |
Beam, V-Notched; Dry; Autoclave Cured; ASTM D5379-93 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 6K 4HS IM7 Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 52.4 MPa @Temperature 163 °C |
7600 psi @Temperature 325 °F |
Short Beam |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |