Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.5195 MPa @Shear Rate 5000 1/s, Temperature 240 °C |
75.35 psi @Shear Rate 5000 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |