Polymer Property : Shear Strength = 7496 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 51.68 MPa

@Temperature 232 °C
7496 psi

@Temperature 450 °F
T300, Plain Weave; Fill Short Beam; Dry
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form
Fiber: T300-3KInformation provided by HexCel