Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 74.5 MPa @Temperature -53.9 °C |
10800 psi @Temperature -65.0 °F |
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 74.5 MPa @Temperature -55.0 °C |
10800 psi @Temperature -67.0 °F |
Fill Short Beam, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Shear Strength | 74.5 MPa @Temperature 104 °C |
10800 psi @Temperature 220 °F |
0° Short Beam, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |