Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.483 MPa @Temperature 107 °C, Time 1.81e+6 sec |
70.0 psi @Temperature 225 °F, Time 504 hour |
Overlap |
3M Scotch-Weld™ 10 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 10 is a multi-purpose contact adhesive which may be used to bond plastic laminate, aluminum, steel, wallboard, wood, masonry, rubber and canvas.Informati.. |
|||
Shear Strength | 0.483 MPa @Temperature 82.0 °C |
70.0 psi @Temperature 180 °F |
Overlap, Plexiglass |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.483 MPa @Temperature 82.0 °C |
70.0 psi @Temperature 180 °F |
Overlap, Plexiglass |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.483 MPa @Temperature 82.0 °C |
70.0 psi @Temperature 180 °F |
Overlap, Plexiglass |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |