Mechanical Properties Metric English Comments
Shear Strength 46.0 MPa

@Temperature 177 °C
6670 psi

@Temperature 351 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric
Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel
Shear Strength 46.0 MPa

@Temperature 22.2 °C
6670 psi

@Temperature 72.0 °F
Lap Shear Primed, 1000 hrs in anti-icing fluid at 72°F
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf)
Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve..
Shear Strength 46.0 MPa

@Temperature 22.2 °C
6670 psi

@Temperature 72.0 °F
Lap Shear Primed, 1000 hrs in hydraulic oil at 72°F
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf)
Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve..
Shear Strength 46.0 MPa

@Temperature 60.0 °C
6670 psi

@Temperature 140 °F
0º Interlaminar Shear, Conditioning: 60°C-90%RH; ASTM D2344
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre
1947 - 38% resin weight with M46J 52.5% fiber volumeInformation provided by HexCel