Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 6530 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 45.0 MPa

@Temperature 177 °C
6530 psi

@Temperature 351 °F
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64%; Wet condition-96 hours in boiling H2O
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber
Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel
Shear Strength 45.0 MPa

@Temperature 23.0 °C
6530 psi

@Temperature 73.4 °F
Interlaminar shear
Hexcel® HexPly® M36/NC2 180°C (350°F) Curing Epoxy Matrix, Multiaxial Fabric Laminate (NC2)
Uses Hexcel NC2 non-crimp fabric based on Tenax HTS fiber; Quasi-isotropic lay-up based on 1072 gsm quadaxial NC2 fabric (267 gsm/ply); Laminates manufactured via resin film infusionInformation prov..
Shear Strength 45.0 MPa

@Temperature 23.0 °C
6530 psi

@Temperature 73.4 °F
Short Beam Shear, Dry; EN2563
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound
HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ..
Copyright © lookpolymers.com All Rights Reserved